Stainless steels the most common: austenitic

Austenitic stainless steel is the (stainless steel), the most commonly used. Property belonging to this line can prompt the steel grade SUS 301, stainless steel 304, 304L, 316 stainless steel, 316L, 321, 310S … this to take the minimum 7% nickel, 16% chromium, carbon (C) 12:08% max . Similar components created for this steel corrosion resistant high temperature in the framework of general relativity, not magnetized, flexible, malleable and easy to weld. This steel is used to make various household appliances, containers, industrial hose, industrial ships, exterior architecture, cultivating other works …
thep-khong-gi
Type Stainless steel identifiable as soft mechanical: ferritic

Ferritic stainless steel is the (stainless steel) have similar physical properties mild steel, but with corrosion resistance higher than mild steel (steel carbonthap). This form of ownership belong to mention the steel grade SUS 430, 410, 409 … This kind of brings contains about 12% – 17% chromium. This line, carrying 12% Cr diversity often applied in architecture. what to take about 17% Cr is used to make furniture, pot pretty, washing machine, indoor architecture …

Stainless steel type and nature of austenitic ferritic: Duplex

Austenitic ferritic-(Duplex) This is a stainless steel with nature “in the middle” ferritic and austenitic form of ownership is the common name DUPLEX. This property belongs to remind the LDX 2101, SAF 2304, 2205, 253MA. duplex steels with Ni containing less popular than bearing the austenitic. DUPLEX with typical features are high strength and durability of ordinary soft used in the petrochemical industry, the supply of paper, pulp, manufactured marine vessels … Given the escalating price of stainless steel anhydrous nickel are rare due to the DUPLEX is increasingly wider application to replace the first number of the steel austenitic steels such as SUS 304, 304L, 316, 316L, 310S …

See more : Aluminum plate and Copper busbar

Inox stainless steel General Directorate: Martensitic

Martensitic units contain about 11% to 13% Cr, bearing durability and low hardness, corrosion resistance at a level quite. Used to manipulate various blades, blades …

SUMMARY
SUS 430: contamination between, prone to the effects of the environment that marred
SUS 202: magnetic, prone to the influence of the environment makes marred
SUS 201: No contamination in the range (99%), durable carrying period, but avoid direct contact with acid or salt.
SUS 304: nonmagnetic, consumables ownership in any environment, shiny, ensure food safety.
SUS 316: no contamination between, ownership can be used in any environment, said both environments require very strict cleanliness